Test report of 200D UHMWPE Fiber in 2008

10D-200D UHNWPE Fiber

The test sample is 200D/60F UHMWPE fiber in original white color and test by CTTC in 2008 and the tenacity was 31.7cN/dtex.

Tested ItemResultStandard
Linear Density222dtex
Breaking Tenacity31.7cN/dtexISO 2062-1993
CV of breaking tenacity6.57%
Breaking elongation3.18%
CV of breaking elongation8.55%
*The test results are transferred from below Chinese version.

Part view of UHMWPE fiber test report – 200D/60F